CF8M is the designation in both the ACI and ASTM systems for this material. J92900 is the UNS number. It has a fairly high ductility and a moderately high thermal conductivity among cast austenitic stainless steels. The graph bars on the material properties cards below compare ACI-ASTM CF8M steel to: cast austenitic stainless …
astm a351 gr. cf8m Valves have up to 21% chromium and 8% nickel in their chemical composition with carbon, manganese, silicon, sulfur, phosphorus and molybdenum in the …
CF8M is a cast austenitic material for pressure containing parts, which covered by ASTM A351 and ASTM A743 and ASTM A744 standard. CF8M Chemical Requirements in …
Stainless steel butterfly valve materials are mainly divided into 304, 316, 304L, 316L and other stainless steel materials.However, the material on the valve body does often appear CF8, CF8M, CF3, CF3M and so on.. There are many customers because it is written on the contract that it is a butterfly valve: DN50, 304, 20 sets.
Overview. CF8M / 316 stainless steel is a modification of 304 stainless steel with the addition of 2.0% to 3.0% molybdenum to provide improved resistance to reducing corrosives and pitting attack by chlorides as found in seawater. Careful balance of the chemical composition strengthens this alloy to levels well above most specifications.
CF8M is a chromium-nickel-molybdenum alloy with high resistance to oxidation and pitting corrosion. It has excellent resistance to chlorides and other chemical environments. …
Cast Alloy Designation: CF8M. Similar designation: AISI 316. Alloy Family: High Alloy / Stainless Steel. UNS #: J92900. ASTM Standard (s): A351/A743/A744. Wrought: 316. …
The austenitic stainless steel casting grade CF8M is the most extensively used in the US. In this article, you will learn the properties of CF8M material, applications, and alternatives. The ASTM A351 Standard Specification provides guidance for austenitic castings for pressure-containing parts. The ASTM 743 and ASTM A744 standard
ASTM A351 gr. CF8M Stainless Steel (316 equivalent) ASTM A351 gr. CF3M Low Carbon Stainless Steel (316L equivalent) ASTM A351 gr. CF8 Stainless Steel (304 equivalent) ASTM A351 gr. CF3-304L Low Carbon Stainless Steel (304L equivalent) ASTM A351 gr. CN7M-Alloy 20 ASTM A296 gr. CW-12M Hastelloy C ASTM A296 gr. M-35 Monel ASTM …
Physical Properties of steel grade ASTM CF8M. Temperature. (°C) Modulus of elasticity. (GPa) Mean coefficient of thermal expansion 10-6/ (°C) between 20 (°C) and. Thermal conductivity. (W/m·°C)
astm a182 f316/f316l astm a351 cf8m/cf3m astm a182 f321 astm a182 f347 astm a351 cf8c astm a182 f44 (6mo) astm ck3mcun astm a182 f20* (alloy 20) a351 cn7m ferritic-austenitic stainless steel astm a182 f51 - uns s31803† (duplex s.s.) astm a995* gr.4a/a351 cd3mn astm a182 f53 - uns s32750 (super duplex s.s.) astm a995* gr.5a/a351 ce3mn
CF8M is a cast austenitic material for pressure containing parts, which covered by ASTM A351 and ASTM A743 and ASTM A744 standard. CF8M Chemical Requirements in those three standards as …
CF8M stainless steel is the most widely used US standard austenitic stainless steel casting grade. Its equivalent type is cast 316. From the name CF8M, the letter "C" means the alloy is mainly for the purpose of corrosion resistance. The letter "F" is the approximate location on the iron-chromium-nickel (FeCrNi) ternary diagram.
CF8M is a versatile austenitic stainless steel that offers good corrosion resistance and strength. It has excellent weldability and formability, making it a popular choice for many applications. UNS Number of Cf8M Material is J92900. The CF8M material specification covers the chemical and mechanical requirements for this grade of stainless …
Stainless steel SA-351 CF8M is a molybdenum bearing modification of CF8 austenitic steel alloy and is the cast equivalent of wrought AISI 316 stainless steel. The presence of …
astm a351 cf8/cf8m (stainless steel) The ASTM A351 specification covers austenitic steel castings for valves, flanges, fittings, and other pressure-containing parts. The most …
The CF-8M is a cast version of wrought AISI Type 316 SS. As far as replacement, it depends on your specific application. jsummerfield (Electrical) 22 Dec 04 11:57. There are a few similar material references that you may be able to find. In addition to AISI you will find cast type 316 Stainless Steel references as ASTM A351 Grade CF8M …
ASTM A351 Standard Specification for Castings, Austenitic, Austenitic-Ferritic (Duplex), for Pressure-Containing Parts1. This specification covers austenitic steel castings for valves, flanges, fittings, and other pressure-containing parts. The steel shall be made by the electric furnace process with or without separate refining such as argon-oxygen …
ASTM A351 CF8 & CF8M are the common cast stainless steel grades in all the stainless steel foundries. They are similar, but not complete the same. Specialised in stainless …
ASTM A351 CG8M. An austenitic stainless steel classified in ASTM under A351 for Castings, Austenitic, for Pressure-Containing Parts. UNS# J93000
The chemical composition of stainless steel can be divided into two broad categories: austenitic and ferritic. While CF8M and CF3M are part of the austenitic family, they also differ in their composition. The main component that sets them apart from each other is chromium content; CF8M contains 8-10% chromium, while CF3M contains 3-4%.
CF8M is defined in ASMT A351, ASMT A743 and ASTM A744, which is for casting purpose only. SS316 is defined in ASTM A240 and ASTM A276, it's for plate, sheet, strip or stainless steel bars. Another grade is named as F316, which is from ASTM A182 for Forged parts only. TP316 will be found in
CF8 Stainless Steel Casting. AISI 304 or CF8 stainless steel castings means the casting parts made of CF8 stainless steel. It is a general grade, belonging to austenitic stainless steel. It is widely used in the foundry industry. The standard composition of CF8 stainless steel is 18% chromium plus 8% nickel. It is non-magnetic.
TABLE 2 Chemical Requirements NOTE 1—Tungsten is a new element for Table 2. Element, % (max, ex-cept where range is given) CF3, CF3A CF8, CF8A CF3M, CF-3MA …
astm a351 cf8/cf3: astm a182 f316/f316l: astm a351 cf8m/cf3m: astm a182 f347: astm a351 cf8c: astm a182 f321: astm a182 f44 (6mo) astm ck3mcun: astm a182 f20* (alloy 20) astm a351 cn7m: ferritic-austenitic stainless …
TABLE 2 Chemical Requirements NOTE 1—Tungsten is a new element for Table 2. Element, % (max, ex-cept where range is given) CF3, CF3A CF8, CF8A CF3M, CF-3MA CF8M CF3MN CF8C CF10 CF-10M (J92-901) CH8 CH10 CH20 CK20 HK30 HK40 HT30
ASTM A351 CF8M. Austenitic stainless steel classified for Castings, Austenitic, for Pressure-Containing Parts. UNS# J92900
As with CF8M, the first character (C) means the alloy is intended for "Corrosion Resistant" service. The second character (F) is the approximate location on the iron-chromium-nickel (FeCrNi) ternary diagram and indicates the iron, chromium and nickel content. A351 CF8M. A351 CG3M. A351 CG8M. A351 CH20. A351 CK20. A351 CK3MCUN. A351 …
CF8M, Disc: ASTM A351 GR. CF8M, Seat: EPDM, Spring: SS316, CLASS Rating: 150. End: Suitable for mounting between ASMEB 16.5, Qty: 1 Nos. Note for all items: (1). All applicable test certificate shall be provided along with the offer. (2) The supply shall be subjected to inward inspection at BHEL site and after
A forged valve body is produced by forging and machining solid steel. The key specifications for cast steel valves body materials are ASTM A216 (WCA, WCB, WCC), ASTM A352 LCB/LCC (low …